1 viewer
Sedimentary · Carbonate
Tufa
tufaCool springs and lake shores.
- Grain
- Fine
- Dry density
- 1.6 t/m³
- From its mineralsThe density worked from the minerals by volume share, less the pore space. The catalogue holds the stated figure within 5% of this one.
- 1.63 t/m³
- Pore space
- 40%
- StrengthUnconfined compressive strength of an intact piece. A jointed rock mass is far weaker.
- 8 MPa
What it is made of
Hand specimenThe colour is that of a common fresh piece. Hardness by share is the minerals' Mohs hardness by volume: a guide to tool wear, not to strength.
- Colour
- rgb(214, 204, 180)
- Hardness by share
- Mohs 3.08